ASACLEAN grade · PP low residue

ASACLEAN newUPLow-residue grade for PP

Low-residue grade for PP jobs, PE-compatible per terms

Helps color or material change in PP jobs with easy system purging-out. Fits jobs controlling residue, including transparent or unreinforced PP resins

Download TDSSelect grades for PPCompare all grades
170–300°COperating temperature
Technical fit

When to choose newUP

For PP jobs needing low residue, or as post-NewEX chaser in PP jobs per TDS and site terms

Process
Injection including Hot Runner; extrusion profile, sheet, blown film and compounding
Resin
PP-based resins; usable with PE
Hot Runner
Compatible with minimum 0.5 mm clearance
Glass Fiber
Glass-fiber-free
Shutdown / Sealing
Supported
Residence Time
Max 30 min residence above 280°C
Use sequence

Safe use

Verify actual temperature, clearance and screen mesh before use. Screens must be no finer than 100 mesh, and purge out per TDS steps before starting the next resin production

Related grades

Compare with nearby grades

UP UP is the standard grade for PP CP CP is the cost-side option for PP/PE; newUP targets low residue

newUP FAQ

Can newUP run Hot Runner

Yes, with minimum 0.5 mm passage, and the real system terms must be checked before use

Can newUP run PE

Yes per TDS data — but the primary pick should follow the job type: PE film and sheet may fit UF2 better, and PE blow molding may fit UB better

Plan a newUP trial on PP jobs

Send PP type, temperature, machine, Hot Runner and site problems for technician term checks

LINE

Compare PP options

Compare UP, newUP and CP by cleaning goal Verify terms before entering transparent PP jobs

LINE